GRP · glass reinforced plastic

GRP fibreglass roofing in Leeds

A fibreglass roof is made on the spot: matting is wetted out with resin on a new deck and sets into one hard, seamless skin. Done in the right conditions on the right boards, it gives crisp edges and a tough surface.

GRP Fibreglass Roofing in Leeds

Leave your name and number and the office will phone you back.

Calls are returned in office hours. Or ring 0113 460 1042.

GRP Fibreglass Roofing across Leeds

GRP stands for glass reinforced plastic. On a roof it means a layer of chopped glass-fibre matting bonded into polyester resin over a timber deck, finished with a pigmented topcoat that protects it from sunlight. Because it is laminated in place, it flows round corners, up kerbs and over edges without a joint, which makes it a good fit for roofs with detail: balconies, small parapets, dormers and roofs that people walk on.

The quality of a GRP roof depends heavily on the day it is laid. Resin needs dry weather and a sensible temperature to cure properly. Laid on a damp deck, in drizzle or on a cold late afternoon, it can stay tacky, fail to bond or craze later. A good fibreglass roofer would rather move the job than rush it, and that is how we plan it.

It also needs the right deck. GRP is rigid, so it relies on a stable base, normally OSB3 boards with joints taped to allow for movement. Laid over old, damp or springy boards, it tends to crack along board joints.

Signs a fibreglass roof needs work

  • Fine hairline cracks running in straight lines, often along the board joints beneath
  • Crazing or a dusty, faded surface where the topcoat has worn thin
  • Edge trims cracking or coming loose from the laminate
  • A soft or delaminated area that sounds hollow when tapped
  • Water sitting in one area and leaving a stained ring
  • Cracking at internal corners or where the roof meets a wall

What causes GRP roofs to fail

Deck movement

If the boards were not taped at the joints, or the deck is not firm enough, normal movement concentrates at the joints and cracks the laminate above them.

Laid in poor conditions

Damp boards or cold, wet weather during laying leads to poor curing and weak bonding, which can show up months later.

Too little resin or matting

A laminate that is too thin, or matting not fully wetted out, leaves dry spots that let water in.

Topcoat worn away

The topcoat protects the laminate from ultraviolet light. Once it has worn through in places, the layer beneath starts to break down.

Seeing any of this on your roof?Phone, send the form or upload a photo. We look first and then price it in writing.
Ask for a call backPhoto check

How a GRP roof is laid

1. A firm, dry deck

New boards, usually OSB3, are fixed to the joists with the falls set out. Joints are taped so the laminate can cope with small movements.

2. Trims first

GRP edge trims are fixed around the perimeter, ready to be laminated in.

3. Laminate

Resin is rolled onto the deck, glass-fibre matting is laid into it and wetted out, then rolled to remove air. Corners, upstands and trims are bonded in the same skin.

4. Topcoat

Once the laminate has cured, it is lightly prepared and a pigmented topcoat is applied, with a non-slip finish where people will walk.

5. Finish the details

Flashings are fitted where the roof meets a wall, outlets are checked, and the surface is inspected for any dry spots before we leave.

Where GRP sits against EPDM and felt

GRP fibreglassEPDM rubberReinforced felt
Edges and cornersMoulded into one hard skinFolded and bonded sheet, with trimsDressed and bonded layers
Walkable surfaceHard-wearing; can be made non-slipMaintenance traffic; pads for walkwaysOccasional foot traffic
ColourChoice of topcoat coloursBlackMineral colours
Laying conditionsDry, not too cold, for curingDry deck for adhesivesDry surface; works in cooler weather
Typical faultsCracks over deck joints if the deck movesLifted edges and detailsCracked laps and blisters on older roofs

Not sure which suits your roof? The material chooser asks five questions and shows how each one fits.

Worth knowing

Smell on the day

Polyester resin has a strong smell while it cures. It fades, but windows near the roof are best kept shut during laying, and we will warn neighbours where they are close.

Good for balconies

Because GRP can be finished with a hard, non-slip surface, it is often chosen for small balconies and walk-on areas, provided the structure is designed for the loading.

Colour can fade

Topcoats weather slowly. A roof that is overlooked a lot may be re-topcoated in later years to freshen it; that is maintenance, not a sign of failure.

Repairs are visible

A repaired patch of GRP is strong and watertight, but rarely an exact colour match on a weathered roof.

Related flat roof work

Where we do this

Everywhere in the Leeds district. Pages for places where this work comes up a lot: Roundhay, Chapel Allerton, Horsforth, Headingley, Boston Spa, Collingham. For anywhere else, type your town or postcode into the area finder.

GRP Fibreglass Roofing: questions people ask

  • Neither is better in every case. GRP gives a hard, seamless surface and handles detailed shapes and walk-on areas well. EPDM is quicker to lay in mixed weather and very forgiving of temperature. For a plain garage either works well; for a balcony or a roof with many corners, GRP often has the edge. The material chooser on this site walks through the questions.
  • Straight cracks usually follow the joints in the boards below, which means the deck has moved more than the laminate can take. Random crazing often points to a worn topcoat or poor curing. The cause decides the repair: cracks over a moving deck tend to come back unless the deck is dealt with.
  • On mild, dry days, yes. Resin needs suitable temperatures and a dry deck to cure, so winter jobs are planned around the forecast. If the weather turns, the job moves rather than being rushed.
  • GRP needs a stable timber deck, and old felt is not a suitable base. The felt is stripped and new boards are fitted, which also lets us check and replace any soft timber.
  • Topcoats come in a range of colours, with grey the most common on houses. Some people match a dormer to the slates or choose a lighter shade to reflect heat. Colour is agreed in writing with the price.

Want a seamless fibreglass roof?

We check the structure, plan the laying around the weather and put the price in writing first.

Office openUntil 5pm
Call
0113 460 1042
Ask for
a price